Hastelloy C22/C276 Pipes & Tubes
Hastelloy C22/C276 Seamless Welded Pipes | ASME SB622 Hastelloy UNS N06022/N10276 Seamless & Welded Pipes & Tubes
Hastelloy C22/C276 Seamless Welded Tubes |Hastelloy C22/C276 Pipes And Tubes Manufacturer
Jainex Metal is a prestigious association that is moderately occupied with offering an extensive variety of Hastelloy C22/C276 Pipes and Tubes. It is by and large considered the most flexible warmth safe and erosion safe amalgam accessible. Alloy C22/C276 offers incredible imperviousness to setting, stress-corrosion breaking, and high temperature airs. Furthermore, because of its low carbon content, it opposes the development of grain limit encourages in the weld-influenced zone making it helpful for applications in the as-welded condition.
We offer these UNS N06022/N10276 Pipes and Tubes in global and national nature of benchmarks at financially savvy rates to our supporters. As a maker, supplier, stockiest and exporter, we offer these Hastelloy Alloy C22/C276 Pipes and Tubes in uniquely designed sizes and thicknesses according to the accurate requests of our regarded customers.
Specification Of Hastelloy C22/C276 Seamless Welded Pipes Tubes
Standard |
ASTM & ASME |
Size |
½”NB – 24”NB |
Schedule |
SCH 10 – SCH XXS |
Grade |
ASTM B 729 , 829 , 468 , 751 , 464 , 775 , 474 ASME SB 729 , 829 , 468 , 751 , 464 , 775 , 474 |
Type |
Seamless / ERW / Welded / Fabricated / LSAW Pipes |
Form |
Round, Square, Rectangular, Hydraulic Etc. |
End |
Plain End, Bevelled End, Threaded |
Length |
Single Random, Double Random & Cut Length |
Chemical Composition of Hastelloy C22
Element |
Min |
Max |
Molybdenum |
12.5 |
14.5 |
Chromium |
20.0 |
22.5 |
Iron |
2.00 |
6.00 |
Tungsten |
2.50 |
3.50 |
Cobalt |
-- |
2.50 |
Carbon |
-- |
0.010 |
Silicon |
-- |
0.08 |
Manganese |
-- |
0.50 |
Vanadium |
-- |
0.35 |
Phosphorus |
-- |
0.025 |
Sulfur |
-- |
0.010 |
Chemical Composition of Hastelloy C276
Element |
Min |
Max |
Molybdenum |
15.0 |
17.0 |
Chromium |
14.5 |
16.5 |
Iron |
4.0 |
7.0 |
Tungsten |
3.0 |
4.5 |
Cobalt |
-- |
2.50 |
Manganese |
-- |
1.0 |
Carbon |
-- |
0.1 |
Vanadium |
-- |
0.35 |
Phosphorus |
-- |
0.04 max |
Sulfur |
-- |
.03 max |
Silicon |
-- |
.08 max |
Mechanical Properties
Grade |
Tensile (ksi) |
.2% Yield (ksi) |
Elongation % |
Hardness (HRb) |
C22 |
115 |
55 |
60 |
89 |
C276 |
110 |
52.6 |
62 |
- |
Physical Properties of Hastelloy C22
Density |
0.314 lb/in3 |
Specific Gravity |
8.69 lb/in3 |
Specific Heat (Btu/lb/Deg F - [32-212 Deg F] |
0.1 |
Melting Point (Deg F) |
2550 |
Thermal Conductivity |
70 |
Mean Coeff Thermal Expansion |
6.9 |
Modulus of Elasticity Tension |
29.9 |
Physical Properties of Hastelloy C276
Physical Property |
Temp., °F |
British Units |
Temp., °C |
Metric Units |
Density |
72 |
0.321 lb/in.3 |
22 |
8.89 g/cm.3 |
Melting Range |
2415-2500 |
|
1323-1371 |
|
Electrical Resistivity |
75 |
51 microhm-in. |
24 |
1.30 microhm-m |
Mean Coefficient of
Thermal Expansion |
75-200 |
6.2 microinches/in.-°F |
24-93 |
11.2 x 10-6 m/m•K |
75-400 |
6.7 microinches/in.-°F |
24-204 |
12.0 x 10-6 m/m•K |
75-600 |
7.1 microinches/in.-°F |
24-316 |
12.8 x 10-6 m/m•K |
75-800 |
7.3 microinches/in.-°F |
24-427 |
13.2 x 10-6 m/m•K |
75-1000 |
7.4 microinches/in.-°F |
24-538 |
13.4 x 10-6 m/m•K |
Thermal Conductivity |
-270 |
50 Btu-in./ft.2 hr.-°F |
-168 |
7.2 W/m•K |
-100 |
60 Btu-in./ft.2 hr.-°F |
-73 |
8.6 W/m•K |
0 |
65 Btu-in./ft.2 hr.-°F |
-18 |
9.4 W/m•K |
100 |
71 Btu-in./ft.2 hr.-°F |
38 |
10.2 W/m•K |
200 |
77 Btu-in./ft.2 hr.-°F |
93 |
11.1 W/m•K |
400 |
90 Btu-in./ft.2 hr.-°F |
204 |
13.0 W/m•K |
600 |
104 Btu-in./ft.2 hr.-°F |
316 |
15.0 W/m•K |
800 |
117 Btu-in./ft.2 hr.-°F |
427 |
16.9 W/m•K |
1000 |
132 Btu-in./ft.2 hr.-°F |
538 |
19.0 W/m•K |
Specific Heat
(Calculated) |
Room |
0.102 Btu/lb.-°F |
Room |
427 J/kg•K |